Flux de-ironing
In the carbon steel galvanisation process it is important for the flux bath to contain a constant low iron (Fe) concentration. To achieve this a flux de-ironing installation is the most appropriate technique.
In this installation the Fe is oxidised and then discharged via de-watering to obtain a clear flux.
PCA can help you with this technology, both in design and construction of the installation.